1 |
Carbon-induced corrosion of MSF condenser tubes in Arabian Gulf water El Din AMS, El-Dahshan ME, Haggag HH Desalination, 172(3), 215, 2005 |
2 |
Scale formation in flash chambers of high-temperature MSF distillers El Din AMS, El-Dahshan ME, Mohammed RA Desalination, 177(1-3), 241, 2005 |
3 |
Bio-film formation on stainless steels Part 2. The role of seasonal changes, seawater composition and surface roughness El Din AMS, El-Dahshan ME, El Din AMT Desalination, 154(3), 267, 2003 |
4 |
Vapour side corrosion in a ME desalination plant at Jebel Dhana El-Dahshan ME, Al Malek S, Al Katheeri E Desalination, 155(1), 67, 2003 |
5 |
Reverse osmosis incorporated into existing cogenerating systems as a sustainable technological alternative for United Arab Emirates Agashichev SP, El-Dahshan ME Desalination, 157(1-3), 33, 2003 |
6 |
Inhibition of the thermal decomposition of HCO3- - A novel approach to the problem of alkaline scale formation in seawater desalination plants El Din AMS, El-Dahshan ME, Mohammed RA Desalination, 142(2), 151, 2002 |
7 |
Galvanic corrosion in the systems titanium/316 L stainless steel/Al brass in Arabian Gulf water El-Dahshan ME, El Din AMS, Haggag HH Desalination, 142(2), 161, 2002 |
8 |
A new form of titanium condenser tube droplet erosion El-Dahshan ME, Wang LF, El Din AMS, Bin Ashoor B Desalination, 133(2), 149, 2001 |
9 |
Corrosion and scaling problems present in some desalination plants in Abu Dhabi El-Dahshan ME Desalination, 138(1-3), 371, 2001 |
10 |
Dissolution of copper and copper-nickel alloys in aerated dilute HCl solutions El Din AMS, El Dahshan ME, El Din AMT Desalination, 130(1), 89, 2000 |