1 |
Structural development of gel-spinning UHMWPE fibers through industrial hot-drawing process analyzed by small/wide-angle X-ray scattering Xu HJ, An MF, Lv Y, Zhang L, Wang ZB Polymer Bulletin, 74(3), 721, 2017 |
2 |
Biaxial hot-drawing of poly(ethylene terephthalate): An experimental study spanning the processing range Buckley CP, Lew CY Polymer, 52(8), 1803, 2011 |
3 |
PROPERTIES OF UNIAXIALLY STRETCHED POLYPROPYLENE FILMS: EFFECT OF DRAWING TEMPERATURE AND RANDOM COPOLYMER CONTENT Sadeghi F, Tabatabaei SH, Ajji A, Carreau PJ Canadian Journal of Chemical Engineering, 88(6), 1091, 2010 |
4 |
Structure and properties of MDO stretched polypropylene Tabatabaei SH, Carreau PJ, Aji A Polymer, 50(16), 3981, 2009 |
5 |
Structural deformation behavior of isotactic polypropylene with different molecular characteristics during hot drawing process Sakurai T, Nozue Y, Kasahara T, Mizunuma K, Yamaguchi N, Tashiro K, Amemiya Y Polymer, 46(20), 8846, 2005 |
6 |
Hot-drawing of poly(methyl methacrylate) and simulation using a glass-rubber constitutive model Dooling PJ, Buckley CP, Rostami S, Zahlan N Polymer, 43(8), 2451, 2002 |
7 |
In situ study of structure development during continuous hot-drawing of poly(trimethylene terephthalate) fibers by simultaneous synchrotron small- and wide-angle X-ray scattering Wu J, Schultz JM, Samon JM, Pangelinan AB, Chuah HH Polymer, 42(16), 7161, 2001 |
8 |
High speed melt spinning of poly(L-lactic acid) filaments Mezghani K, Spruiell JE Journal of Polymer Science Part B: Polymer Physics, 36(6), 1005, 1998 |
9 |
In-Vitro Degradation of Poly(L-Lactic Acid) Fibers Produced by Melt-Spinning Pegoretti A, Fambri L, Migliaresi C Journal of Applied Polymer Science, 64(2), 213, 1997 |
10 |
Biodegradable Fibers of Poly(L-Lactic Acid) Produced by Melt-Spinning Fambri L, Pegoretti A, Fenner R, Incardona SD, Migliaresi C Polymer, 38(1), 79, 1997 |