검색결과 : 3건
No. | Article |
---|---|
1 |
Radiation damage and Raman vibrational modes of single-walled carbon nanotubes Ritter U, Scharf P, Dmytrenko OP, Kulish NP, Prylutskyy YI, Belyi NM, Gubanov VA, Komarova LA, Lizunova SV, Shlapatskaya VV, Bernas H Chemical Physics Letters, 447(4-6), 252, 2007 |
2 |
Investigation on soaking and formation of lead/acid battery plates with different mass structure Dreier I, Saez F, Scharf P, Wagner R Journal of Power Sources, 85(1), 117, 2000 |
3 |
Electrodeposited, dispersion-hardened, lightweight grids for lead-acid batteries Barkleit G, Grahl A, Maccagni M, Olper M, Scharf P, Wagner R, Warlimont H Journal of Power Sources, 78(1-2), 73, 1999 |