1 |
Suppression of active-oxidation of Si-C fibers (Hi-Nicalon) under reduced pressure by carbon or silica coating Shimoo T, Okamura K, Morita T Journal of Materials Science, 39(5), 1547, 2004 |
2 |
Effect of CO2 partial pressure on oxidation of low-oxygen SiC fibers (Hi-Nicalon) in Ar-CO2 gas mixtures Shimoo T, Okamura K, Morita T Journal of Materials Science, 39(8), 2699, 2004 |
3 |
Carbon elimination by heat-treatment in hydrogen and its effect on thermal stability of polycarbosilane-derived silicon carbide fibers Shimoo T, Katase Y, Okamura K, Takano W Journal of Materials Science, 39(20), 6243, 2004 |
4 |
High temperature exposure of low-oxygen SiC fibers (Hi-Nicalon) in CO-CO2 gas mixtures Shimoo T, Okamura K, Morita T Journal of Materials Science, 39(23), 7031, 2004 |
5 |
Oxidation behavior and mechanical properties of low-oxygen SiC fibers prepared by vacuum heat-treatment of electron-beam-cured poly(carbosilane) precursor Shimoo T, Okamura K, Mutoh W Journal of Materials Science, 38(8), 1653, 2003 |
6 |
Thermal stability of low-oxygen silicon carbide fibers (Hi-Nicalon) in carbon monoxide Shimoo T, Okamura K, Morita T Journal of Materials Science, 38(14), 3089, 2003 |
7 |
Effect of reduced pressure on oxidation and thermal stability of polycarbosilane-derived SiC fibers Shimoo T, Okamura K, Takeuchi H Journal of Materials Science, 38(24), 4973, 2003 |
8 |
Suppression of active oxidation of polycarbosilane- derived silicon carbide fibers by preoxidation at high oxygen pressure Shimoo T, Morisada Y, Okamura K Journal of the American Ceramic Society, 86(5), 838, 2003 |
9 |
Active-to-passive oxidation transition for polycarbosilane-derived silicon carbide fibers heated in Ar-O-2 gas mixtures Shimoo T, Okamura K, Morisada Y Journal of Materials Science, 37(9), 1793, 2002 |
10 |
Oxidation behavior and thermal stability of Si-C-O fibers (Nicalon) in carbon dioxide Shimoo T, Morita T, Okamura K Journal of Materials Science, 37(15), 3181, 2002 |