검색결과 : 1건
No. | Article |
---|---|
1 |
&ITIn situ&IT nanomechanical behavior and self-healing response of polymeric multilayer thin films Humood M, Polychronopoulou K, Song YX, Grunlan JC, Polycarpou AA Polymer, 131, 169, 2017 |
No. | Article |
---|---|
1 |
&ITIn situ&IT nanomechanical behavior and self-healing response of polymeric multilayer thin films Humood M, Polychronopoulou K, Song YX, Grunlan JC, Polycarpou AA Polymer, 131, 169, 2017 |