화학공학소재연구정보센터
검색결과 : 18건
No. Article
1 The hygrothermal aging effects of titanium hydride potassium perchlorate for pyrotechnic combustion
Oh J, Ambekar A, Yoh JJ
Thermochimica Acta, 665, 102, 2018
2 Impact of hygrothermal aging on structure/function relationship of perfluorosulfonic-acid membrane
Shi SW, Dursch TJ, Blake C, Mukundan R, Borup RL, Weber AZ, Kusoglu A
Journal of Polymer Science Part B: Polymer Physics, 54(5), 570, 2016
3 Hygrothermal aging of an adhesive reinforced with microparticles of cork
Barbosa AQ, da Silva LFM, Ochsner A
Journal of Adhesion Science and Technology, 29(16), 1714, 2015
4 Influence of hygrothermal aging on the gas and water transport properties of Nafion (R) membranes
Naudy S, Collette F, Thominette F, Gebel G, Espuche E
Journal of Membrane Science, 451, 293, 2014
5 Mechanical properties of Nafion 212 proton exchange membrane subjected to hygrothermal aging
Shi SW, Chen G, Wang ZF, Chen X
Journal of Power Sources, 238, 318, 2013
6 Fuel cell rejuvenation of hygrothermally aged Nafion (R)
Collette FM, Thominette F, Escribano S, Ravachol A, Morin A, Gebel G
Journal of Power Sources, 202, 126, 2012
7 Effect of Silane Adhesion Promoters on Subcritical Debonding of Epoxy/Glass Interfaces After Hygrothermal Aging
Onjun O, Pearson RA
Journal of Adhesion, 86(12), 1178, 2010
8 Hygrothermal aging of Nafion (R)
Collette FM, Lorentz C, Gebel G, Thominette F
Journal of Membrane Science, 330(1-2), 21, 2009
9 Reliability of Anisotropic Conductive Adhesive Joints in Electronic Packaging Applications
Lin YC, Chen X
Journal of Adhesion Science and Technology, 22(14), 1631, 2008
10 Effects of hygrothermal aging on anisotropic conductive adhesive joints: experiments and theoretical analysis
Lin YC, Chen X, Wang ZP
Journal of Adhesion Science and Technology, 20(12), 1383, 2006