1207 - 1213 |
Kinetics of the Electroreduction of Anodically Formed Cadmium-Oxide Layers in Alkaline-Solutions Deurraza JI, Gervasi CA, Saidman SB, Vilche JR |
1214 - 1222 |
Modeling of the Sodium-Ferrous Chloride Electrochemical-Cell Orchard SW, Weaving JS |
1223 - 1231 |
Analysis of Spontaneous Electrochemical Noise for Corrosion Studies Roberge PR |
1232 - 1236 |
Current Efficiency and Crystallization Mechanism in Pulse Plating of Hard Chromium Leisner P, Bechnielsen G, Moller P |
1237 - 1243 |
Mass-Transport in a Hydrogen Gas-Diffusion Electrode Vermeijlen JJ, Janssen LJ |
1244 - 1250 |
Hydrated Structures in the Anodic Layer Formed on Lead Electrodes in H2SO4 Solution Monahov B, Pavlov D |
1251 - 1258 |
Ceramic Electrodes for an Alkali-Metal Thermoelectric Converter (Amtec) Nakata H, Nagata T, Tsuchida K, Kato A |
1259 - 1262 |
Paired Electrooxidation .2. Production of Anthraquinone in an Undivided Cell Lee AC, Chou TC |
1263 - 1267 |
Measurement of Anode Potentials at High-Current Densities by the Current Interruption Method for Metals Used in Aviation Technology Hives J, Rousar I |
1268 - 1272 |
Behavior of Tungsten Carbide Hydrogen-Diffusion Electrodes in Chloride Etching Solutions Nikolova V, Nikolov I, Vitanov T, Wiesener K |
1273 - 1279 |
An Electrochemical Model for Reduction of MnO2 with Fe2+ Ions Bayramoglu M, Tekin T |
1280 - 1284 |
Electrochemical Passivation of Copper-Aluminum Silver Alloy in Sodium-Hydroxide Solution Kulandainathan MA, Iyer SV, Baba RS, Vasudevan T |
1285 - 1292 |
A Modified Hull Cell with Forced Electrolyte Flow - Simulation of Industrial Electroplating Conditions Degrez M, Duchene A, Fontana A, Winand R |
1293 - 1300 |
Current-Density Optimization in Electrochemical Synthesis Gonet M, Korczynski A |
1301 - 1309 |
Electrochemical Regeneration of Ceric Sulfate in an Undivided Cell Been J, Oloman CW |
1310 - 1316 |
A Model of the Electrochemical-Behavior Within a Stress-Corrosion Crack Li DL, Huang Z |
1317 - 1322 |
Current Efficiency During Anodic-Dissolution of Iron to Ferrate(VI) in Concentrated Alkali Hydroxide Solutions Bouzek K, Rousar I |
1323 - 1325 |
Interfacial Supersaturation at Gas Evolving Electrodes Vogt H |