7717 - 7718 |
Preface to the special issue on ultrafine-grained materials Mathaudhu SN, Huang XX, Kim HS, Langdon TG, Lowe TC, Valiev RZ, Wu XL, Zehetbauer M, Zhu YTT |
7719 - 7725 |
Twenty-five years of severe plastic deformation: recent developments in evaluating the degree of homogeneity through the thickness of disks processed by high-pressure torsion Kawasaki M, Figueiredo RB, Langdon TG |
7726 - 7734 |
Using deformation mechanism maps to depict flow processes in superplastic ultrafine-grained materials Kawasaki M, Langdon TG |
7735 - 7743 |
Bimodal grain size distribution: an effective approach for improving the mechanical and corrosion properties of Fe-Cr-Ni alloys Mahesh BV, Raman RKS, Koch CC |
7744 - 7750 |
Anticorrosion behavior of ultrafine-grained Al-26 wt% Si alloy fabricated by ECAP Jiang JH, Ma AB, Song D, Yang DH, Shi J, Wang KL, Zhang LY, Chen JQ |
7751 - 7758 |
The effect of deformation texture on the thermal stability of UFG HSLA steel Bruder E |
7759 - 7763 |
Thermal stability up to 800 A degrees C of a Ni-4 wt% Al nanocomposite Zheng L, Peng X, Wang F |
7764 - 7769 |
The effect of alloying with hafnium on the thermal stability of chromium bronze after severe plastic deformation Shangina DV, Bochvar NR, Dobatkin SV |
7770 - 7776 |
Mechanical properties and thermal stability of bulk Cu cold consolidated from atomized powders by high-pressure torsion Yoon EY, Lee DJ, Ahn DH, Lee ES, Kim HS |
7777 - 7781 |
Enhanced fatigue properties of ultrafine-grained Ti rods processed by ECAP-Conform Semenova IP, Polyakov AV, Raab GI, Lowe TC, Valiev RZ |
7782 - 7788 |
Achieving homogeneity in a Cu-Zr alloy processed by high-pressure torsion Wongsa-Ngam J, Kawasaki M, Langdon TG |
7789 - 7795 |
Microstructural evolution and the mechanical properties of an aluminum alloy processed by high-pressure torsion Sabbaghianrad S, Kawasaki M, Langdon TG |
7796 - 7806 |
Effect of temperature on the processing of a magnesium alloy by high-pressure torsion Huang Y, Figueiredo RB, Baudin T, Helbert AL, Brisset F, Langdon TG |
7807 - 7814 |
Analysis of plastic flow during high-pressure torsion Figueiredo RB, Aguilar MTP, Cetlin PR, Langdon TG |
7815 - 7820 |
Effect of aging on microstructural development in an Al-Mg-Si alloy processed by high-pressure torsion Loucif A, Figueiredo RB, Kawasaki M, Baudin T, Brisset F, Chemam R, Langdon TG |
7821 - 7827 |
Effects of ball milling and high-pressure torsion for improving mechanical properties of Al-Al2O3 nanocomposites Ashida M, Horita Z |
7828 - 7834 |
Nanoindentation analysis for local properties of ultrafine grained copper processed by high pressure torsion Jeong HJ, Yoon EY, Lee DJ, Kim NJ, Lee S, Kim HS |
7835 - 7840 |
Analysis of microstructure and microhardness of Zr-2.5Nb processed by High-Pressure Torsion (HPT) Companhoni MVP, Matheus JRG, Marcondes TL, Pinto AL |
7841 - 7847 |
Evolution of ultrafine microstructures in commercial purity aluminum heavily deformed by torsion Khamsuk S, Park N, Adachi H, Terada D, Tsuji N |
7848 - 7853 |
Mechanical behavior of nanocrystalline TiNi alloy produced by severe plastic deformation Valiev RZ, Gunderov DV, Lukyanov AV, Pushin VG |
7854 - 7859 |
The activation of aOE (c) c plus a > non-basal slip in Magnesium alloys Kang F, Li Z, Wang JT, Cheng P, Wu HY |
7860 - 7869 |
Microstructure and dislocation density evolutions in MgAlZn alloy processed by severe plastic deformation Janecek M, Cizek J, Gubicza J, Vratna J |
7870 - 7876 |
Microstructure and tensile strength of grade 2 titanium processed by equal-channel angular pressing and by rolling Sordi VL, Ferrante M, Kawasaki M, Langdon TG |
7877 - 7882 |
Deformation behavior of consecutive workpieces in equal channel angular pressing of solid dies Joo SH, Yoon SC, Jeong HG, Lee S, Kim HS |
7883 - 7887 |
The achievement of high strength in an Al 6061 alloy by the application of cryogenic and warm rolling Kang UG, Lee HJ, Nam WJ |
7888 - 7893 |
Microstructure and microtexture evolution in pure metals after ultra-high straining Zhilyaev AP, Langdon TG |
7894 - 7900 |
Microstructural evolution and mechanical behavior of warm multi-axially forged HSLA steel Padap AK, Chaudhari GP, Pancholi V, Nath SK |
7901 - 7907 |
Strain distribution during tensile deformation of nanostructured aluminum samples Kidmose J, Lu L, Winther G, Hansen N, Huang X |
7908 - 7913 |
Plasma nitriding of steels with severely plastic deformed surfaces Schuster J, Bruder E, Muller C |
7914 - 7920 |
Cold rolled nanostructured super-pure Al (99.9996%) containing 1 % Si particles: structure and strength Huang TL, Dong QS, Gong X, Hansen N, Liu Q, Huang XX |
7921 - 7925 |
Dilatometry: a powerful tool for the study of defects in ultrafine-grained metals Sprengel W, Oberdorfer B, Steyskal EM, Wurschum R |
7926 - 7931 |
Nickel with multimodal grain size distribution achieved by SPS: microstructure and mechanical properties Dutel GD, Tingaud D, Langlois P, Dirras G |
7932 - 7938 |
Ultrafine-grained nickel refined by dislocation activities at intermediate strain rate impact: deformation microstructure and mechanical properties Farbaniec L, Abdul-Latif A, Gubicza J, Dirras G |
7939 - 7945 |
Influence of severe plastic deformation on the precipitation hardening of a FeSiTi steel Fillon A, Sauvage X, Pougis A, Bouaziz O, Barbier D, Arruffat R, Toth LS |
7946 - 7953 |
Grain size effect on high-speed deformation of Hadfield steel Ueji R, Kondo D, Takagi Y, Mizuguchi T, Tanaka Y, Shinagawa K |