1501 - 1504 |
Piezoelectric properties of [Bi-0.5(Na0.7K0.25Li0.05)(0.5)]TiO3-Ba(Ti,Zr)O-3 binary system ceramics Zhang ZY, Jia JF, Yang HZ, Chen CQ, Sun HW, Hu X, Yang DL |
1505 - 1509 |
Fabrication and characterization of anisotropic dielectrics for low-loss microwave applications Zhang LL, Mumcu G, Yarga S, Sertel K, Volakis JL, Verweij H |
1510 - 1514 |
Titanate nanotubes: preparation, characterization, and application in the detection of dopamine Niu LL, Shao MW, Wang S, Lu L, Gao HZ, Wang J |
1515 - 1519 |
Improvement of morphology and luminescence of CaS : Eu2+ red-emitting phosphor particles via carbon-containing additive strategy He XH, Zhu Y |
1520 - 1524 |
Thermoelectric properties of perovskite oxides La1-xSrxCoO3 prepared by polymerlized complex method Zhou AJ, Zhu TJ, Zhao XB |
1525 - 1531 |
The effect of the cerium precursor and the carbon surface chemistry on the dispersion of ceria on activated carbon Ramos-Fernandez EV, Serrano-Ruiz JC, Silvestre-Albero J, Sepulveda-Escribano A, Rodriguez-Reinoso F |
1532 - 1538 |
Incorporation of zirconia particles into coatings formed on magnesium by plasma electrolytic oxidation Arrabal R, Matykina E, Skeldon P, Thompson GE |
1539 - 1545 |
Age-hardening behaviour of a spinodally decomposed low-carat gold alloy Park MG, Yu CH, Seol HJ, Kwon YH, Kim HI |
1546 - 1551 |
Microstructure and wear properties of Fe-TiC surface composite coating by laser cladding Qu SY, Wang XH, Zhang M, Zou ZD |
1552 - 1558 |
Light-induced bone cement-philic titanium surface Aita H, Oh W, Kubo K, Tsukimura N, Maeda H, Ogawa T |
1559 - 1567 |
Study on microstructure and properties of Ni-based alloy/Y2O3-deposited metals by laser cladding Xu PQ, Gong HY, Xu GX, He JP, Yu ZS |
1568 - 1575 |
The strain rate and temperature dependence of microstructural evolution of Ti-15Mo-5Zr-3Al alloy Lee WS, Lin CF, Chen TH, Hwang HH |
1576 - 1582 |
Adiabatic shear band in a Ti-3Al-5Mo-4.5V titanium alloy Wang BF |
1583 - 1586 |
High-pressure homogenization treatment of Al-Zn-Mg-Cu aluminum alloy Li H, Cao DH, Wang ZX, Zheng ZQ |
1587 - 1592 |
Proton and oxide-ionic conduction in Sr- and Zn-doped LaGaO3 Zhang F, Sun LL, Zhu JL, Pan B, Xu R, Ma GL |
1593 - 1598 |
Effect of heavy interstitials on anelastic properties of Nb-1.0 wt% Zr alloys de Souza AC, Grandini CR, Florencio O |
1599 - 1611 |
Production and characterization of ZrO2 ceramics and composites to be used for hip prosthesis Arin M, Goller G, Vleugels J, Vanmeensel K |
1612 - 1618 |
Measurement and analytical validation of interfacial bond strength of PAN-fiber-reinforced carbon matrix composites Tezcan J, Ozcan S, Gurung B, Filip P |
1619 - 1623 |
Morphology and luminescent properties of Al3+/Mg2+-doped Y2O3 : Eu3+ phosphor Liu Z, Feng Y, Jiao DM, Zhang N, Jiao H |
1624 - 1629 |
Effect of frequency and duty cycle on corrosion behavior of pulsed nanocrystalline plasma electrolytic carbonitrided CP-Ti Aliofkhazraei M, Rouhaghdam AS, Sabouri M |
1630 - 1637 |
Propene/1-octene copolymers as a new pervaporative membrane material for wastewater treatment Tian XZ, Jiang X |
1638 - 1643 |
Low temperature synthesis of nanocrystalline Sb2Te3 by mechanical alloying Zakeri M, Allahkarami M, Kavei G, Khanmohammadian A, Rahimipour MR |
1644 - 1649 |
Microstructure and magnetic properties of electrodeposited cobalt films Bhuiyan MS, Taylor BJ, Paranthaman M, Thompson JR, Sinclair JW |
1650 - 1663 |
Development of epoxy-based electrets Liu YC, Aoyagi Y, Chung DDL |
1664 - 1668 |
YBCO nanofibers synthesized by electrospinning a solution of poly(acrylic acid) and metal nitrates Greenberg Y, Lumelsky Y, Silverstein MS, Zussman E |
1669 - 1676 |
Photochemical synthesis and characterization of Ag/TiO2 nanotube composites Li HB, Duan XC, Liu GC, Liu XQ |
1677 - 1680 |
Lead-free piezoelectric BNKLT 1-3 composites Lam KH, Guo MS, Lin DM, Kwok KW, Chan HLW |
1681 - 1687 |
Preparation and luminescence performance of rare earth agriculture-used light transformation composites Yang C, Sun ZF, Liu L, Zhang LQ |
1688 - 1695 |
The energy required to ignite micropyretic synthesis. Part I: stable Ni plus Al reaction Li HP |
1696 - 1700 |
Polymer-ITO nanocomposite template for the optoelectronic application Chatterjee S |
1701 - 1710 |
Phase composition and wear behavior of NiTi alloys Gialanella S, Ischia G, Straffelini G |
1711 - 1715 |
ZnO microcolumns originated from self-assembled nanorods Li Y, Li WF, Xu G, Ma XL, Cheng HM |
1716 - 1722 |
Formation of composite Cu-graphite and Cu-PTFE coatings and their tribological characterization Omidvar H, Stremsdoerfer G, Meas Y |
1723 - 1729 |
Modifier ligands effects on the synthesized TiO2 nanocrystals Attar AS, Ghamsari MS, Hajiesmaeilbaigi F, Mirdamadi S |
1730 - 1733 |
Preparation and characterization of ZrO2 porous nanosolid and its composite fluorescent materials Liu XL, Cui DL, Li Y, Guo Y |
1734 - 1739 |
Magnetocaloric effect in La1-xCaxMnO3 for x=0.3, 0.35, and 0.4 Szymczak R, Czepelak M, Kolano R, Kolano-Burian A, Krzymanska B, Szymczak H |
1740 - 1744 |
Experimental Zn-rich corner of the Fe-Zn-Cu ternary phase diagram at 460 degrees C Avettand-Fenoel MN, Hadadi A, Reumont G, Perrot P |
1745 - 1748 |
Viscoelasticity and macromolecular topology in single-site catalyzed polyethylene Vega JF, Polo-Ceron D, Gomez-Ruiz S, Prashar S, Fajardo M, Martinez-Salazar J |