965 - 967 |
Self-Propagating High-Temperature Synthesis (SHS) of Titanium Carbide Mishra SK, Das S, Goel RP, Ramachandrarao P |
968 - 970 |
Preparation and Structure of Bulk Nanostructured WC-Co Alloy by High-Energy Ball-Milling Ma XM, Ling Z, Gang J, Dong YD |
971 - 973 |
Preparation and Structure of the System (Na1-Xlax) (Nb1-(2X/3)Mg2X/3)O-3 with X=0.51, 0.50, 0.435 and 0.4275 Sahu AK, Parkash OM, Kumar D |
974 - 976 |
Effect of Film Thickness on Preferred Growth of Tin Films During Filtered Arc Deposition Zhao JP, Wang X, Chen ZY, Yang SQ, Shi TS, Liu X |
977 - 981 |
Effects of Residual-Stress on R-Curve Behavior of Ceramic-Matrix Composites Deng ZY, Shi JL, Shi Y, Jiang DY, Guo JK |
982 - 984 |
Synthesis and Properties of Spodumene-Modified Mullite Ceramics Formed by Sol-Gel Processing Low IM, Suherman PM, Phillips PN |
985 - 987 |
Characteristics of Carbon-Fiber-Reinforced Calcium-Phosphate Composites Fabricated by Hot-Pressing Park K, Vasilos T |
988 - 990 |
Partial Melting During Formation of YBa2Cu3O7-X Chen JH, Besser MF, Trivedi RK, Kramer MJ, Sordelet DJ |
991 - 992 |
Iridium Distributions in Silicate Glass for Sedimentology Studies Vance ER, Carter ML, Blackford MG |
993 - 995 |
Bearing Failure in Plain Woven C/C Composites Tsuda H, Takahashi J |
996 - 998 |
Photoinduced Decomposition of Platinum Metalorganic Films for Electroless Copper Plating Zhang JY, Boyd IW |
999 - 1001 |
High-Pressure Synthesis of C-60-Containing Polystyrene Kojima Y, Matsuoka T, Takahashi H, Kurauchi T |
1002 - 1004 |
Plasma-Sprayed ZrO2-Sm2O3 Coatings - Lattice-Parameters, Tetragonality (C/A) and Transformability of Tetragonal Zirconia Phase Khor KA, Yang J |
1005 - 1007 |
Diamond Formation from the B4C-Fenico System at High-Temperature and High-Pressure Luo XJ, Qiang L, Ding LY, Luo BC |
1008 - 1011 |
Kinetic Fracture of Glass at the Nanometer-Scale Henaux S, Creuzet F |
1012 - 1016 |
Microstructure of Alpha-AgI-Frozen Composites in the AgI-Ag2O-B2O3 System After Heat-Treatment Torata N, Saito T, Tatsumisago M, Minami T |
1017 - 1019 |
Towards Particle-by-Particle Deposition of Ceramics Using Electrostatic Atomization Teng WD, Huneiti ZA, Machowski W, Evans JR, Edirisinghe MJ, Balachandran W |
1020 - 1022 |
Temperature Stable Dielectric-Properties for Pb(Mg1/3Nb2/3)O-3-BaTiO3-PbTiO3 System Ceramics Ruan LJ, Li LT, Gui ZL |
1023 - 1026 |
Alumina Composite Membranes Prepared by MOCVD Ha HY, Lee JS, Nam SW, Kim IW, Hong SA |
1027 - 1029 |
Evaluation of Epoxy Underfill Materials for Solder Flip-Chip Technology Park CE, Han BJ, Bair HE, Raju VR |
1030 - 1032 |
Diffusion Joining of Si3N4 Ceramics by Hot-Pressing Under High-Nitrogen Gas-Pressure Nakamura M, Shigematsu I |
1033 - 1036 |
Formation of Lamellar Structure in Gamma-Titanium Aluminide Chang JY, Moon I, Choi C |
1037 - 1039 |
Luminescence Efficiency of SnO2-Eu and Rate of SnO Oxidation Maneva N, Kynev K, Grigorov L, Lijutov L |
1040 - 1042 |
Size Distribution of Large Grain-Boundary Cracks in the Creep-Ruptured Specimens of a Cobalt-Based Alloy Tanaka M |
1043 - 1044 |
Coating-Substrate Bonding After Hvof Thermally Spraying WC-Co on to a Ti-6-Percent-Al-4-Percent-V Alloy Guilemany JM, Nutting J, Dong Z |
1045 - 1047 |
Optically Transparent and Nonlinear LiNbO3 - Polyimide Composite - Preparation and Characterization Tripathi AK, Roy A, Goel TC, Pillai PK, Singh K |
1048 - 1050 |
Suppression of Ignition and Burning of Molten Mg Alloys by Ca Bearing Stable Oxide Film Sakamoto M, Akiyama S, Ogi K |
1051 - 1054 |
Nonequilibrium W-Cu System Alloy Powder and Bulk Body Prepared by Mechanical Alloying and Shock Compression Mashimo T, Huang XS, Tashiro S |