화학공학소재연구정보센터

Journal of Materials Science Letters

Journal of Materials Science Letters, Vol.17, No.23 Entire volume, number list
ISSN: 0261-8028 (Print) 

In this Issue (23 articles)

1953 - 1955 The effect of strain rate on the interfacial fracture properties of carbon fiber-metal laminates
Reyes G, Cantwell WJ
1957 - 1959 Evaluation of the characteristics of La(Co1-xAlx)O-3 as possible SOFC cathodes
Hrovat M, Bernik S, Kuscer D, Holc J, Kolar D
1961 - 1962 Composite model for creep behaviors of pure aluminums at a room temperature
Ishikawa K, Okuda H, Kobayashi Y
1963 - 1965 A study of the factors affecting surface insulation resistance measurements
Sarkar G, Chong YF, Collier PA
1967 - 1969 Toughening mechanism of Ni3Al alloys by B-doping
Inoue M, Suganuma K, Niihara K
1971 - 1973 Range of metastability of tetragonal zirconia in some rare earth doped zirconia fibers
Naskar MK, Ganguli D
1975 - 1977 "Universal" response of hopping carriers
Jonscher AK
1979 - 1981 Hydrothermal modification of pre-sintered barium titanate powders
Voltzke D, Abicht HP, Woltersdorf J, Pippel E
1983 - 1985 Spectroscopic study of amorphous precursors for alkaline-earth titanates and stannates
Pfaff G, Hildenbrand VD, Fuess H
1987 - 1990 Microstructure and fracture toughness of Si3N4 based ceramics subjected to pre-sinter heat treatments
Plucknett KP, Lewis MH
1991 - 1993 Internal friction in Y-TZP ceramic
Shepel SV, Drapkin BM
1995 - 1997 Electron beam evaporation of nickel manganite thin-film negative temperature coefficient thermistors
Parlak M, Hashemi T, Hogan MJ, Brinkman AW
1999 - 2001 Chemical preparation and properties of semi-metal BaPbO3 ceramics
Kodama Y, Murayama N, Torii Y, Yasukawa M
2003 - 2005 Tensile properties of the ZK60 magnesium alloy produced by hot extrusion of machined chip
Nakanishi M, Mabuchi M, Saito N, Nakamura M, Higashi K
2007 - 2008 Glass formation and physicochemical properties of the GeSe2-Sb2Se3Ag2Se(ZnSe) systems
Vassilev VS, Boycheva SV, Ivanova ZG
2009 - 2011 Fatigue behavior of a copper tricrystal - Part I Cyclic deformation and crack initiation
Jia WP, Li SX, Wang ZG, Li GY
2013 - 2015 Influence of Al layers on the work function of SnO2-based gas sensors
Farag ESM, Abo-Ghazala MS
2017 - 2019 Effect of trace elements on eutectic carbide morphology during heat treatment
Wang SQ, Jiang QC, Chui XH, He ZM
2021 - 2023 The influence of chromium and boron on mechanical properties of Fe-30Al alloy
Su JQ, Gao SJ, Hu ZQ
2025 - 2027 Effect of annealing on the hyperfine field distributions in Fe79B16Si5 and Fe78B13Si9 metallic glasses
Bandyopadhyay D, Singru RM
2029 - 2031 Three-zone liquid metals solidification model
Bakhtiyarov SI, Overfelt RA
2033 - 2035 A new method for fabrication of functionally gradient materials
Huang JH, Li JF, Akira K, Ryuzo W
2037 - 2040 Lamp-induced forward transfer: a new approach for deposition of metal films
Zhang JY, Boyd IW, Esrom H