Przemysl Chemiczny, Vol.93, No.4, 453-456, 2014
Thermal cutting of porous polymers
Expanded polystyrene plates (100 mm thick) were cut with moving resistance wires (diam. 0.16-0.34 mm, speed 150-600 mm/min) to det. the effect of current intensity and power supply on cutting gap. The increase in the wire heating power and the wire diam. as well as the decrease in the wire cutting speed resulted in an increase in the width of the cutting gap.