Korean Journal of Materials Research, Vol.22, No.7, 374-378, July, 2012
3D패키지용 Via 구리충전 시 전류밀도와 유기첨가제의 영향
Effects of Current Density and Organic Additives on via Copper Electroplating for 3D Packaging
E-mail:
In an effort to overcome the problems which arise when fabricating high-aspect-ratio TSV(through silicon via), we performed experiments involving the void-free Cu filling of a TSV(10~20 μm in diameter with an aspect ratio of 5~7) by controlling the plating DC current density and the additive SPS concentration. Initially, the copper deposit growth mode in and around the trench and the TSV was estimated by the change in the plating DC current density. According to the variation of the plating current density, the deposition rate during Cu electroplating differed at the top and the bottom of the trench. Specifically, at a current density 2.5 mA/cm2, the deposition rate in the corner of the trench was lower than that at the top and on the bottom sides. From this result, we confirmed that a plating current density 2.5 mA/cm2 is very useful for void-free Cu filling of a TSV. In order to reduce the plating time, we attempted TSV Cu filling by controlling the accelerator SPS concentration at a plating current density of 2.5 mA/cm2. A TSV with a diameter 10 μm and an aspect ratio of 7 was filled completely with Cu plating material in 90 min at a current density 2.5 mA/cm2 with an addition of SPS at 50 mg/L. Finally, we found that TSV can be filled rapidly with plated Cu without voids by controlling the SPS concentration at the optimized plating current density.
  1. Kondo K, Yonezawa T, Mikami D, Okubo T, Taguchi Y, Takahashi K, Barkey DP, J. Electrochem. Soc., 152(11), H173 (2005)
  2. Yang Y, Labie R, Ling F, Zhao C, Radisic A , Van Olmen J, Travaly Y, Verlinden B, De Wolf I, Microelectron. Reliab., 50, 1636 (2010)
  3. Tan M, Harb JN, J. Electrochem. Soc., 150(6), C420 (2003)
  4. Wang ZL, Yaegashi O, Sakaue H, Takahagi T, Shingubara S, J. Electrochem. Soc., 151(12), C781 (2004)
  5. Radisic A, Luhn O, Philipsen HGG, El-Mekki Z, Honore M, Rodet S, Armini S, Drijbooms C, Bender H, Ruythooren W, Microelectronic Eng., 88, 701 (2011)
  6. Delbos E, Omnes L, Etcheberry A, Microelectronic Eng., 87, 514 (2010)
  7. Song Y, Seo JH, Lee YS, Rha SK, Kor. J. Mater, Res., 19(6), 334 (2009)
  8. Woo TG, Park IS, Lee HW, Seol KW, Kor. J. Mater, Res., 16(11), 710 (2006)
  9. Wang W, Li YB, Li YL, Appl. Surf. Sci., 255(8), 4389 (2009)
  10. Dow WP, Li CC, Su YC, Shen SP, Huang CC, Lee C, Hsu B, Hsu S, Electrochim. Acta, 54(24), 5894 (2009)
  11. Gallaway JW, Willey MJ, West AC, J. Electrochem. Soc., 156(8), D287 (2009)
  12. Noh SS, Choi EH, Lee YH, Ju HJ, Rha SK, Lee BJ, Kim DK, Lee YS, in Proceedings of the 18th IEEE International Symposium on the Physical and Failure Analysis of Integrated Circuits(Incheon, Korea, July, 2011) p. 305. (2011)
  13. Chang GH, Lee JH, J. Microelectron. Packag. Soc., 13(4), 45 (2006)