Korean Journal of Materials Research, Vol.21, No.9, 477-481, September, 2011
카본블랙 첨가 PMC(Polyethylene Matrix Composites)의 문턱스며들기(Percolation Threshold)와 절연파괴 강도 임계지수
Percolation Threshold and Critical Exponent of Dielectric Breakdown Strength of Polyethylene Matrix Composites added Carbon Black
E-mail:
Composites of insulating polyethylene and carbon black are widely used in switching elements, conductive paint, and other applications due to the large gap of resistance value. This research addresses the critical exponent of dielectric breakdown strength of polymer matrix composites (PMC) made with carbon black and polyethylene below the percolation threshold (Pt) for the first time. Here, Pt means the volume fraction of carbon black of which the resistance of the PMC is transferred from its sharp decrease to gradual decrease in accordance with the increase of carbon-black-filled content. First, the Pt is determined based on the critical exponents of resistivity and relative permittivity. Although huge cohesive bodies of carbon black are formed in case of being less than the Pt, a percolation path connecting the conducting phases is not formed. The dielectric breakdown strength (Dbs) of the PMC below Pt is measured by using an impulse voltage in the range from 10 kV to 40 kV to avoid the effect of joule heating. Although the observed Dbs data seems to be well fitted to a straight line with a slope of 0.9 on a double logarithm of (Pt-VCB) and Dbs, the least squares method gives a slope of 0.97 for the PMC. It has been found that finite carbon-black clusters play an important role in dielectric breakdown.
- Nakamura S, J. Inst. Electrostat. Jpn., 25(3), 142 (2001)
- Sichel EK, Carbon Black-polymer Composites, p. 253-280, ed. Sichel EK, Mercel Dekker, New York, USA (1982)
- Probst N, Conductivity Imparted by Carbon Black to Composites, p. 273, ed. Donnet JB, Bansel RC, Wang MJ, Marcel Dekker, New York, USA (1993). (1993)
- Shin SG, Met. Mater. Int., 7(6), 519 (2001)
- Shin SG, Lim HJ, Lee JH, Kor. J Mater. Res., 13(11), 732 (2003)
- Stauffer D, Aharony A, Introduction to Percolation Theory, p. 123-153, Tayler & Francis, London (1992). (1992)
- Shin SG, Korean J. Mater. Res., 20(5), 271 (2010)
- Shin SG, Electron. Mater. Lett., 6(2), 65 (2010)
- Shin SG, Kor. J. Met. Mater., 48(9), 867 (2010)
- Miyasaka K, Watanabe K, Jojima E, Aida H, Sumita M, Iishikawa K, J. Mater. Sci., 17, 1610 (1982)
- Mizutani T, Handbook of Electronic Materials, p. 637-640, ed. Kimura T, Asakurasyoten, Tokyo, (2006) (in Japanese). (2006)
- Ehrburger-Dolle D, Lahaye J, Misono S, Carbon, 32(7), 1363 (1994)
- Webman I, Jortner J, Cohen MH, Phys. Rev. B, 16(6), 2593 (1977)
- Efros AL, Shklovskii BI, Phys. Status Solidi B, 76, 475 (1976)
- Ohtsuki T, Keyes T, J. Phys. Math. Gen., 17, L559 (1984)
- Niemeyeer L, Pietronero L, Wiesman HJ, Phys. Rev. Lett., 52(12), 1033 (1985)
- Takayasu H, Phys. Rev. Lett., 54(11), 1099 (1985)
- Tanamoto T, Toriumi A, Jpn. J. Appl. Phys., 36(3B), 1439 (1997)
- Beale PD, Duxbury PM, Phys. Rev. B, 37(6), 2785 (1988)
- Shin SG, Korean J. Mater. Res., 19(12), 644 (2009)