Crack behavior of Surface Strengthened Zirconia-Alumina Composite During Indentation
E-mail:
ZTA tubes were prepared by centrifugal casting and sintered at for 2 hrs. The ZTA tubes were machined into specimens of mm. Molten Soda lime glass (SLG) was penetrated into the surface of ZTA at an optimized condition of for the holding time of 5 h and furnace cooled. The extra glass on the surface was removed using a resin bonded diamond wheel. The glass penetrated samples were tested for their flexural strength using four point bend test. Vickers Indentation cracks were made on the glass penetrated surface at different loads of 9.8 N, 49 N, 98 N and 196 N. The residual compression on the surface enhanced the flexural strength and crack arrest behaviour remarkably. This was attributed to the thermoelastic mismatch between the glass and ZTA matrix during cooling.
  1. Kingery WD, Bowen HK, Uhlmann DL, Introduction to Ceramics. Ch. 16, Second edition. John Wiley & Sons, New York (1976) (1976)
  2. Tandon RR, Green DJ, Cook R, J. Am. Ceram. Soc., 73, 2619 (1990)
  3. Green DJ, Tandon R, Sglavo VM, Science, 283(5406), 1295 (1999)
  4. Kirchner HP, Gruver RM, Walker RE, J. Am. Ceram. Soc., 51, 251 (1968)
  5. Noda S, Doi H, Hioki T, Kawamoto JI, Kamigaito O, J. Am. Ceram. Soc., 69, C210 (1986)
  6. Virkar AV, Huang HW, Cutler RA, J. Am. Ceram. Soc., 70, 164 (1987)
  7. Green DJ, J. Am. Ceram Soc., 66, C178 (1983)
  8. Chu MC, Cho SJ, Yoon KJ, Park HM, J. Am. Ceram. Soc., 88(2), 491 (2005)
  9. Jhcbarocn J, Padmre NP, J. Am. Ceram. Soc., 81, 2301 (1998)
  10. Balakrishnan A, Chu MC, Panigrahi BB, Yoon KJ, Kim JC, Lee BC, Kim TN, Cho SJ, Sol. Stat. Phenom., 124, 1161 (2006)
  11. Volf MB, Mathematical Approach to Glass (Elsevier Science Publishers, USA 1988) (1988)
  12. Cullity BD, Elements of 'X-ray' Diffraction (Addison Wesley Publishing Co., Inc., Reading, Massachusetts, USA 1978 (1978)
  13. Paranjpye AG, Beltz E, MacDonald NC, Modelling Simulation Mater. Sci. Eng., 13, 329 (2005)
  14. Luo J, Stevens R, J. Eur. Ceram. Soc., 17, 1565 (1997)
  15. Luo J, Stevens R, J. Eur. Ceram. Soc., 22, 159 (2002)
  16. Guazzato M, Albakry M, Ringer, SP, Swain MV, Dent. Mater., 20(5), 441 (2004)