Macromolecular Research, Vol.26, No.11, 1048-1051, November, 2018
Effect of Ozone Treatment on Fracture Toughness of Single-Walled Carbon Nanotubes-Reinforced Epoxy Resin Initiated by a Thermal Latent Catalyst
E-mail:
- Stankovich S, Dikin DA, Dommett GH, Kohlhaas KM, Zimney EJ, Stach EA, Piner RD, Nguyen ST, Ruoff RS, Nature, 442, 282 (2006)
- Balazs AC, Emrick T, Russell TP, Science, 314, 1107 (2006)
- Wan JT, Bu ZY, Xu CJ, Li BG, Fan H, Thermochim. Acta, 519(1-2), 72 (2011)
- Park SJ, Heo GY, Suh DH, J. Polym. Sci. A: Polym. Chem., 41(15), 2393 (2003)
- Ham YR, Lee DH, Kim SH, Shin YJ, Yang M, Shin JS, J. Ind. Eng. Chem., 16(5), 728 (2010)
- Chen MC, Hourston DJ, Schafer FU, Huckerby TN, Polymer, 36(17), 3287 (1995)
- Che BD, Nguyen LTT, Nguyen BQ, Nguyen HT, Le TV, Nguyen NH, Macromol. Res., 22(11), 1221 (2014)
- Azeez AA, Rhee KY, Park SJ, Hui D, Compos. Part B: Eng., 45, 308 (2013)
- Gojny FH, Wichmann MH, Fiedler B, Kinloch IA, Bauhofer W, Windle AH, Schulte K, Polymer, 47, 2036 (2006)
- Treacy MM, Ebbesen TW, Gibson JM, Nature, 381(6584), 678 (1996)
- Wong EW, Sheehan PE, Lieber CM, Science, 277(5334), 1971 (1997)
- Poncharal P, Wang ZL, Ugarte D, de Heer WA, Science, 283(5407), 1513 (1999)
- Kamalakaran R, Terrones M, Seeger T, Kohler-Redlich P, Ruhle M, Kim YA, Hayashi T, Endo M, Appl. Phys. Lett., 77, 3385 (2000)
- Jin Z, Zhang ZQ, Meng LH, Mater. Chem. Phys., 97(1), 167 (2006)
- Valdes H, Sanchez-Polo M, Rivera-Utrilla J, Zaror CA, Langmuir, 18(6), 2111 (2002)
- Mawhinney DB, Naumenko V, Kuznetsova A, Yates JT, Liu J, Smalley RE, J. Am. Chem. Soc., 122(10), 2383 (2000)
- Park SJ, Jin SY, J. Colloid Interface Sci., 286(1), 417 (2005)
- Park SJ, Kim BJ, Mater. Sci. Eng. A-Struct. Mater. Prop. Microstruct. Process., 408, 269 (2005)
- Yuan J, Ma LP, Pei S, Du J, Su Y, Ren W, Cheng HM, ACS Nano, 7, 4233 (2013)
- Xu ZW, Yue MY, Chen L, Zhou BM, Shan MJ, Niu JR, Li BD, Qian XM, Chem. Eng. J., 240, 187 (2014)
- Vennerberg DC, Quirino RL, Jang Y, Kessler MR, ACS Appl. Mater. Interfaces, 6, 1835 (2014)
- Park SJ, Jin FL, Lee JR, Macromol. Rapid Commun., 25(6), 724 (2004)
- Morio K, Murase H, Tsuchiya H, Endo T, J. Appl. Polym. Sci., 32, 5727 (1986)
- Park SJ, Kim TJ, Lee JR, J. Polym. Sci. B: Polym. Phys., 38(16), 2114 (2000)
- Park SJ, Seo MK, Lee JR, Lee DR, J. Polym. Sci. A: Polym. Chem., 39(1), 187 (2001)
- Kim YC, Park SJ, Lee JR, Polym. J., 29, 759 (1997)
- Park SJ, Jin FL, Polym. Degrad. Stabil., 86, 515 (2004)
- Park SJ, Jin FL, Lee JR, Shin JS, Eur. Polym. J., 41, 231 (2005)
- Park SJ, Heo GY, Lee JR, Shim SY, Suh DH, Polym. Korea, 25(4), 558 (2001)
- Cohen A, Yan QL, Shlomovich A, Aizikovich A, Petrutik N, Gozin M, RSC Adv., 5, 106971 (2015)
- Shen SY, Chen JC, Liu SH, Chang RH, Liaw HJ, Shu CM, J. Thermanal. Calorim., 113, 1619 (2013)
- Cools P, Sainz-Garcia E, Geyter ND, Nikiforov A, Blajan M, Shimizu K, Alba-Elias F, Leys C, Morent R, Plasma Process. Polym., 12, 1153 (2015)
- Khare KS, Khare R, J. Phys. Chem. B, 117(24), 7444 (2013)
- Tang LC, Wan YJ, Yan D, Pei YB, Zhao L, Li YB, Wu LB, Jiang LX, Lai GQ, Carbon, 60, 16 (2013)
- Choi KE. Seo MK, Carbon Lett., 14, 58 (2013)
- Wang R, Li Z, Liu W, Jiao W, Hao L, Yang F, Compos. Sci. Technol., 87, 29 (2013)