Journal of the American Ceramic Society, Vol.102, No.12, 7347-7354, 2019
Warm-white light performance of Dy3+, Eu3+: NaLa(WO4)(2) phosphors excited with a 450-nm LED
Dy3+, Eu3+: NaLa(WO4)(2) phosphors are successfully synthesized through the solid-state reaction technique. The phase-structure and morphology are measured via X-ray diffraction and energy dispersive spectrometry. The concentrations of Dy3+, Eu3+, La3+, and W6+ are measured via ICP. The absorption and excited spectra are presented, which indicate that a blue band ranging from 430 to 480 nm is suitable for excitation. Using a commercial blue LED with a wavelength of 450 nm as the excitation light source, emission spectra for samples with varying dopant concentration ratios of Dy(3+ )to Eu3+ are obtained, which show good tunable yellow and red emission. For the purpose of investigating white LED performance, CIE spectra and a white light photo are also presented. The results reveal that varying the dopant concentration ratio of Dy(3+ )to Eu3+ plays a key role in the warm-white performance. With increasing concentration of Eu3+, the correlated color temperature decreases from 4069 to 3172 K, which indicates good warm-white performance.