International Journal of Hydrogen Energy, Vol.45, No.38, 19280-19290, 2020
Study on solid waste pyrolysis coke catalyst for catalytic cracking of coal tar
Low value solid waste pyrolysis coke was used as a catalyst to catalytically crack gas-phase tar to improve tar yield and gas production. Pyrolysis coke with different pyrolysis final temperature and pyrolysis time were prepared, the effect of tar cracking products was studied, and the optimal pyrolysis coke were screened. The pyrolysis coke catalyst was characterized by BET, FTIR, SEM. The results show that the optimal preparation final temperature of pyrolysis coke is 750 degrees C, and the optimal preparation pyrolysis time is 2 h. Compared with the pyrolysis of raw coal, the tar cracking rate increased by 9.3%, after added the pyrolysis coke catalyst, the gas increased by 23.2%, and the light component increased to 36.6%. And the OH, C-N and C-O-C functional groups present on coke are the factors that affect the catalytic cracking. (C) 2020 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.