화학공학소재연구정보센터
Thin Solid Films, Vol.458, No.1-2, 179-185, 2004
Photoluminescence intensity enhancement of ion-doped CdWO4 thin films prepared with pulsed laser deposition
Samarium-, nickel- and cesium-ion doped CdWO4 thin films as well as non-doped CdWO4 thin films were prepared by the pulsed laser deposition (PLD) method. The film thickness and the substrate temperature during PLD were changed to study the role of doped ions on the CdWO4 lattice. The crystalline CdWO4 thin films were obtained by PLD on glass substrates at 1073 K. The CdWO4 (002) XRD signal was more intense on the non-doped, Sm- and Ni-doped PLD films. When the substrate temperature was increased to 1273 K, the peak decreased in intensity, and the (111) peak became more intense than the intensity of the (002) on the ion-doped PLD films whereas the (020) signal was still significant on the non-doped thin film. Photoluminescence spectra were deconvoluted into three components at 2.82, 2.54 and 2.27 eV The contribution of the yellow PL component at 2.27 eV was relatively high on the doped PLD films prepared at 1073 K. However, the overall PL spectra features on PLD films prepared at 1273 K were almost the same as the (010) single crystal surface. Photoluminescence intensities on the PLD films prepared at 1273 K were significantly intense and exceeded that on the CdWO4 (010) single crystal surface. (C) 2003 Elsevier B.V. All rights reserved.