Journal of Colloid and Interface Science, Vol.294, No.1, 69-78, 2006
Surface modification of crosslinked poly(styrene-divinyl benzene) micrometer-sized particles of narrow size distribution by ozonolysis
Micrometer-sized polystyrene template particles of narrow size distribution were prepared by dispersion polymerization of styrene in 2-methoxyethanol. Uniform micrometer-sized poly styrene/crosslinked poly(styrene-divinyl benzene) composite particles were formed by a single-step swelling process of the template particles with styrene, divinyl benzene and benzoyl peroxide, followed by polymerization at 70 degrees C. Uniform micrometer-sized crosslinked poly(styrene-divinyl benzene) particles of higher surface area were produced by dissolution of the template polystyrene part of the former composite particles with N, N-dimethyl form amide. Hydroperoxide conjugated crosslinked poly(styrene-divinyl benzene) particles were produced by ozonolysis of these particles. The effect of ozonolysis conditions, such as exposure time and flow rate of the ozone, on the hydroperoxide conjugation to the crosslinked particles was also studied. Functionalization of the crosslinked poly(styrene-divinyl benzene) particles was performed by graft polymerization of vinylic monomers such as acrylonitrile and chloromethyl styrene on the hydroperoxide conjugated crosslinked particles. This was accomplished by raising the temperature (e.g., 70 degrees C) of deairated acetonitrile dispersions containing the hydroperoxide conjugated particles and the vinylic monomers. The influence of various polymerization parameters on the grafting yield, e.g., monomer concentration, conjugated hydroperoxide concentration, and temperature, was also elucidated. (c) 2005 Elsevier Inc. All rights reserved.
Keywords:surface-modification;microspheres;polystyrene;template;composite;single-step swelling;Crosslinking;ozonolysis;hydroperoxide;grafting