Thin Solid Films, Vol.508, No.1-2, 256-259, 2006
Local wet-oxidation characteristic of strained-Si/SiGe-on-insulator
We have applied wet oxidation to the isolation and gate oxidation of strained-Si/SiGe-on-insulator (SGOI) wafers. Wet oxidation of Si0.8Ge0.2 at 700 degrees C proceeds 30 times as fast as the oxidation rate of strained-Si and without forming a Ge condensed layer behind (SiGC)O-2. P-channel metal-oxide-semiconductor field-effect transistors (MOSFETs) on 15% Ge strained-Si/SGOI wafers were fabricated using wet oxidation to simultaneously form the (SiGe)O-2 field oxide and the gate SiO2. Transconductance was found to be enhanced by 50% when compared with unstrained SOI devices. (c) 2005 Elsevier B.V. All rights reserved.