Advanced Materials, Vol.24, No.10, 1328-1332, 2012
Polarization-Induced Charge Distribution at Homogeneous Zincblende/Wurtzite Heterostructural Junctions in ZnSe Nanobelts
Homogeneous heterostructural wurtzite (WZ)/ zincblende (ZB) junctions are successfully fabricated in ZnSe nanobelts. Polarity continuity across the ZB/WZ interface is demonstrated. The saw- tooth- like potential profile induced by spontaneous polarization across the WZ/ZB/WZ interfaces is identified directly at the nanoscale. The polarization- induced charge distribution across the homogeneous heterostructural interfaces is proposed as a viable alternative approach towards charge tailoring in semiconductor nanostructures.