화학공학소재연구정보센터
학회 한국고분자학회
학술대회 2007년 가을 (10/11 ~ 10/12, 일산킨텍스)
권호 32권 2호
발표분야 기능성 고분자
제목 Surface properties of HMDSO plasma treated polyethylene terephthalate (PET)
초록 The plasma polymer films were deposited from hexamethyldisiloxane (HMDSO) on polyethylene terephthalate (PET) under different operating conditions such as r. f. power ranging from 50W to 400W as well as at different HMDSO/O2 flow ratio. From the surface profilometer and AFM study, the highest deposition rate 38.88 nm/min was found when the substrate was treated for 15 min at r. f. of 200W and HMDSO/O2 flow were 1gm/hr and 12 sccm respectively and the roughness was increased when the samples were treated for a longer time. From FT-IR data, the Si-O-Si bending peak at (820-800) cm-1, the strong Si-O-Si stretching absorption band at (1150-1000) cm-1, the symmetric bending in Si-CH3 at (1270-1260) cm-1 were found but the Si-CH3 bending peak were not found in the spectra for r. f. of 300W and 400W because high plasma power decrease the carbon content and increase the inorganic character. The contact angles were decreased when the r. f. power increased.
저자 모이눌, 김동주, 김원호, 김성룡
소속 충주대
키워드 plasma; HMDSO; PET
E-Mail