제목 The degradation characteristics of intermittent operation using an electrode for alkaline electrolysis
초록 Renewable energy provides an intermittent operation environment, so the electrodes of water electrolysis need high durability and long life time for hydrogen production. In this study, 3-electrode system prepared using NiZnFe electrodes plated under two different conditions and the degradation characteristics of the electrode were confirmed by the cathodic potential on/off test in the hydrogen generation evolution reaction. The on/off test was operated about 150 cycles in the range of about -1.3 V to 0 V and reverse current occurred in the off step. As a result of LSV(Linear sweep voltammetry) for electrochemical analysis, the HER activity of 80 mA/cm2, 2000 s electrode and 320 mA/cm2, 2000 s electrode decreased about 10% and 15%, respectively. This results show that Zn dissolution and reverse current are related to deactivation. 320 mA/cm2, 600 s electrode is relatively less deactivation and less peeling off coating layer than 80 mA/cm2, 2000 s electrode.
저자 한지민1, 김종원1, 배기광1, 박주식1, 정성욱1, 김영호2, 강경수1
소속 1한국에너지기술(연), 2충남대
키워드 Intermittent operation; alkaline electrolysis
E-Mail