Assessment of remaining life of superheater austenitic steel tubes in oil shale PF boilers Klevtsov I, Tallermo H, Bojarinova T, Dedov A Oil Shale, 23(3), 267, 2006 |
2 |
Laboratory tests of high-temperature corrosion of steels B-407, X8CrNiNb1613 and X8CrNiMoNb1616 under impact of ash formed at pulverized firing of oil shale Tallermo H, Klevtsov I, Bojarinova T, Dedov A Oil Shale, 22(4), 467, 2005 |
3 |
High-temperature corrosion resistance of the austenitic steels in the presence of chlorine-containing on-tube deposits Klevtsov I, Tallermo H, Bojarinova T, Lausmaa T Oil Shale, 20(4), 501, 2003 |