1037 - 1040 |
Highly Conductive P-Type Microcrystalline Silicon-Carbide Prepared by Photochemical Vapor-Deposition Dasgupta A, Ghosh S, Ray S |
1041 - 1042 |
Dielectric Composite Ceramics in Ba(Mg1/3Ta2/3)O-3-Baond(2)O(3)5Tio(2) System Chen XM |
1043 - 1045 |
Pole Figure Studies in Melt Grown Y-Ba-Cu-O Samples Gopalan R, Singh AK, Rajasekharan T, Rangarajan G, Varadaraju UV |
1046 - 1047 |
Fabrication of Silicon-Nitride Nano-Ceramics by Spark Plasma Sintering Nishimura T, Mitomo M, Hirotsuru H, Kawahara M |
1048 - 1051 |
Correlation Between Microstructure and Gauge Factors of Thick-Film Resistors Hrovat M, Drazic G, Holc J, Belavic D |
1052 - 1054 |
Influence of Boric-Acid Concentration on Silicon-Carbide Morphology Cerovic LJ, Milonjic SK, Bibic NM |
1055 - 1057 |
Study of the Application of Viscous Plastic Processing to Hydroxyapatite Shaw JH, Best SM, Bonfield W, Marsh A, Cotton J |
1058 - 1061 |
Evaluation of Fracture-Toughness of Microalloyed Steel with a Spiked Crack Front Shanmugam P, Pathak SD |
1062 - 1064 |
Application of Diamond-Like Carbon Coatings Deposited by Plasma-Assisted Chemical-Vapor-Deposition Onto Metal-Matrix Composites for 2-Stroke Engine Components Tither D, Ahmed W, Sarwar M, Ahmed E |
1065 - 1067 |
Strengthening and Toughening Behavior of SiC with Additions of TiB2 Yoon JD, Kang SG |
1068 - 1070 |
Crystallization Inhibitors During Sintering of Pyrex Borosilicate Glass Jean JH, Kuan TH, Gupta TK |
1071 - 1073 |
Synthesis of LaCrO3 by the Hydrazine Method Kikkawa T, Yoshinaka M, Hirota K, Yamaguchi O |
1074 - 1077 |
Combustion Synthesis and Properties of Fine-Particle Li-Zn Ferrites Suresh K, Patil KC |
1078 - 1081 |
Densification and Characteristics of Tin Ceramics Graziani T, Bellosi A |
1082 - 1084 |
Structural-Properties Dependent on the Different Lattice-Constants for CdTe and ZnTe Thin-Films Grown on GaAs by Temperature-Gradient Vapor Transport Deposition Kim TW, Park HL |
1085 - 1088 |
Strontium-Barium-Titanate Thin-Films by Sol-Gel Processing Nazeri A, Kahn M, Kidd T |
1089 - 1091 |
Corrosion of Ultimet and 310Ss in a Simulated Waste Incineration Environment 750-Degrees-C Jegede A, Vasantasree V, Hocking MG |
1092 - 1094 |
Thermal Treatments of as-Extruded Eutectoid Zn-21.2Al-1.9 Wt-Percent-Cu Alloy Negrete J, Torres A, Torresvillasenor G |
1095 - 1098 |
Properties of Copper-Aluminum Nitride Composites .2. Rele SV, Raman RV, Unni CK |