1925 - 1926 |
Effect of Single Impact Damage on Strength of Alumina and Zirconia-Toughened Alumina Huang XG, Tu MJ |
1927 - 1931 |
Microstructure and Mechanical-Properties of SiC Particle-Reinforced Al2O3 Matrix Composites Zhang YF, Deng ZY, Shi JL, Mao YQ, Guo JK |
1932 - 1934 |
The Phase-Equilibrium of Binary MgO-Phosphate and CaO-Phosphate Glasses Sahar MR, Kamaruddin N |
1935 - 1937 |
Development of Mechanical-Stress in Sputtered Cr3Si Films During Annealing Bruckner W, Weise G, Mattern N, Reiss G |
1938 - 1939 |
Internal-Stresses in Chromium Phosphorus Electrodeposits Martyak NM, Mccaskie JE, Voos B, Plieth W |
1940 - 1941 |
Catalytic Reduction of No with Co over an Rh/Al Pillared Clay Catalyst Philippopoulos C, Gangas N, Papayannakos N |
1942 - 1944 |
Hydriding Characteristics of Terbium and Rhodium Intermetallics Kulshreshtha SK, Jayakumar OD |
1945 - 1948 |
On Analytical Approaches to the 3-Dimensional Stress State in a Single-Fiber Pull-Out Specimen Leroy FH |
1949 - 1952 |
A Positron-Annihilation Lifetime Spectroscopy Study of Porous Silicon Using a Continuous Lifetime Fitting Algorithm Derlet PM, Choy TC |
1953 - 1955 |
Change of Basic Crystalline Configuration of Blown Polyethylene Induced by a High-Energy Electron-Beam Bernabeu E, Boix JM, Barba C |
1956 - 1959 |
Nitridation of Silicon Under High-Carbon Activity Rao RR, Roopa HN, Kannan TS |
1960 - 1962 |
Grain-Growth of Dense Si-C-N/Additive and SiC at High-Temperatures Kaiser A, Vassen R, Stover D |
1963 - 1965 |
Preloading Technique in Dynamic Fatigue Testing of Ceramics - Effect of Preloading on Strength Variation Choi SR, Salem JA |
1966 - 1968 |
Effect of Interfacial Reaction on the Youngs Modulus of Aluminum Borate Whisker-Reinforced Aluminum Composite Fei WD, Jiang XD, Li C, Yao CK |
1969 - 1972 |
The Effect of Drawing Parameters on the Orientation Distribution in Cross-Linked High-Density Polyethylene Tubing Samburski G, Narkis M, Siegmann A |
1973 - 1975 |
Synthesis of Polytitanates from Ba(Oh)(2)-TiO2-H2O System Through Gel to Crystallite Conversion Kutty TR, Padmini P |
1976 - 1978 |
Crack Healing in Silicon-Nitride and Alumina Ceramics Mitomo M, Nishimura T, Tsutsumi M |
1979 - 1981 |
The Flow Behavior of a Potassium Palmitate Gel-Based Composite Manoharan M |
1982 - 1985 |
Magnetic-Properties of the Triple Perovskite-Rock-Salt Intergrowth Cuproplumbates Ba4-Xpb3-Xcuxo10-Delta (X-Less-Than-or-Equal-to-0.33, Delta-Less-Than-or-Equal-to-0.60) - Evidence of Anomalous Cu2+-O-Pb4+-O-Cu2+ Clustering Bobrysheva N, Chezhina N, Mouron P, Choisnet J |
1986 - 1989 |
An Energy Method to Evaluate Toughening in Ceramics Barinov SM |
1990 - 1993 |
Room-Temperature Strength and Fracture-Toughness of Beta-Sialon(Z=0.5)Center-Dot-SiC Composite Fabricated from Alpha-Si3N4, Aluminum-Isopropoxide and Beta-SiC Kishi K, Umebayashi S |
1994 - 1996 |
Amorphous Alloy-Films Deposited by Excimer-Laser Ablation Using Sintered Ta-Ni Targets Yano T, Ooie T, Yoneda M, Katsumura M |
1997 - 1999 |
Optical Kerr-Effect Observed in a Novel Vanadium Phthalocyanine and Analysis of Its Decay Dynamics Shen YQ, Ling Q, Zhang LX, Zhai JF, Ping Y, Xia ZJ, Zou YH |
2000 - 2001 |
High-Resolution Electron-Microscopy Study of Nickel Silicide - Silicon Interface Grown by Molecular-Beam Epitaxy Feng YZ, Wu ZQ |
2002 - 2007 |
A Characterization of High-Temperature Creep Fracture Life for Ceramics Yokobori AT, Yokobori T, Yamazaki K |
2008 - 2011 |
Anomalous Specific-Heat and Other Properties of Amorphous Ba1-Xlixbio3-Delta(X=0-0.7) Oxides Around Semiconductor-Metal-Semiconductor Like Transition Banerjee G, Sadhukhan M, Bera AK, Karar M, Chaudhuri BK |
2012 - 2015 |
Preparation of Lithium Aluminate Monolith of Controlled Porosity by a Sol-Gel Method Jung JM, Park SB |