Przemysl Chemiczny, Vol.92, No.10, 1788-1791, 2013
Dynamic cross-linking of linear low-density copolymers of ethylene
CH2=CH2/CH2=CHEt and CH2=CH2/CH2=CH(CH2)(6)Me copolymers were crosslinked with (PhCMe2O)(2) initiator (0,2 and 0,5%) at 140-200 degrees C and rotor speed 20 or 60 rpm. A decrease of mol. mass of the copolymers and their melt flow index (esp. at low concn. of initiator) was obsd.