Kunststoffe-Plast Europe, Vol.89, No.8, 86-89, 1999
No cracks - Study of the stress-cracking resistance of housing materials
Styrene copolymers, polycarbonate and polycarbonate blends yield different results when tested for stress-cracking resistance. ASA containing pure acrylic rubber offers the best performance.